Accelerator racks now pull more power than the electrical rooms built for them, and the bill lands on the board. Data centre electricity use sat at about 415 TWh in 2024, roughly 1.5% of global consumption, and the International Energy Agency projects around 945 TWh by 2030 in its base case (Energy and AI). Racks specified at 10 to 15 kW a few years ago now ship above 100 kW, and the high-speed PCB​ inside them has grown to 28 layers or more, with local HDI and thousands of amperes of current.
Ultra-low-loss laminate solves the decibel budget and does nothing for the degree budget. It cuts dielectric loss in the fastest channels, but it is still a glass-reinforced resin that conducts heat at 0.3 to 0.4 W/mK, about three orders of magnitude worse than copper. No laminate grade rescues an overheated server on its own. What works is assigning each layer the material that matches the limit it actually faces.
The rest comes down to telling those two limits apart before the stackup is frozen.

Why AI server boards run into two limits at once
Power density sets both limits on the same board. The signal budget asks how many decibels a channel loses per inch at a given rate. The thermal budget asks how many watts arrive per square centimetre and what temperature the dielectric survives.
Layer count is the visible symptom: 28 to 40 layers, blind and buried vias where routing is dense, copper measured in hundreds of microns near the dies. Every layer adds an interface that must survive reflow and years of cycling, while the stackup holds 100 Ω differential impedance inside a band tight enough for 112G PAM4.
The two limits fail in different ways, so they need separate decisions.
| Signal limit | Thermal limit | |
|---|---|---|
| What sets it | Df, Dk, copper roughness, via stub length | Device power, copper area, cooling capacity |
| How it is measured | dB per inch at the Nyquist frequency | Degrees at the hottest via or bond line |
| What fixes it | Laminate grade, backdrill, impedance control | Copper geometry, thermal vias, substrate change |
| What failure looks like | Closed eye, link downshifted | Delamination, barrel crack, throttle |
Most of the watts on an AI board leave the packages, not the resin. Dielectric loss adds some, but the board’s main job is to carry device heat out, and the dielectric sits in the path.
What ultra-low loss actually buys you
It buys the dielectric term and only the dielectric term. Insertion loss splits into conductor loss and dielectric loss, and a lower Df shrinks the second one while leaving the first untouched.
Dielectric loss scales with frequency, with Df, and with the square root of Dk. Conductor loss scales with the square root of frequency and then worsens for a reason unrelated to resin: at 28 GHz the skin depth in copper is roughly 0.4 µm, the same order as the surface roughness of the foil. A profile measured in microns forces current through a longer path than the trace geometry suggests, and that penalty is set at the copper shop, not the laminate press.
| Grade | Df at 10 GHz | Rate ceiling | Relative cost | Where it belongs |
|---|---|---|---|---|
| Standard FR-4 | 0.015 to 0.020 | About 10 Gbps | Baseline | Consumer boards |
| High-Tg FR-4 | 0.012 to 0.016 | 25 Gbps | Small premium | Power, ground, structural layers |
| Mid-loss FR-4 | 0.008 to 0.010 | 25 to 56 Gbps | Moderate premium | Line cards and switches |
| Low-loss laminate | Around 0.004 | 56 to 112 Gbps | High premium | SerDes and backplane layers |
| Ultra-low-loss | Below 0.002 | 112 Gbps and up | Highest | Longest channels only |
Values shift with glass style, resin content and method, so read them as class ranges rather than part numbers.
Reading the Df number correctly
A Df figure without a frequency is close to meaningless. Suppliers quote at 1 GHz, 10 GHz or 28 GHz, and the same material drifts across that span. Fixtures differ too: a split post dielectric resonator measures a bare coupon, while a stripline measurement includes copper and plating effects.
Compare Df at the frequency your channel runs at, and only against results from the same method. A 1 GHz figure checked against a 28 GHz measurement is how a compliant-looking stackup ends up needing a retimer. Dk needs the same care: a tolerance of plus or minus 0.05 eats a meaningful share of an eight percent impedance band before etch variation is counted.
Where the loss curve goes flat
Below a Df of roughly 0.002, the return on material spend collapses. Conductor loss, via stubs and connectors take over the channel budget, and what remains of dielectric loss is too small a share to pay for.
Three ceilings sit in the way. The conductor floor comes first: once Df is low enough, copper and foil profile dominate and no resin change touches them. Glass weave comes second, because bundles and windows in the fabric create local Dk differences that appear as skew between the two legs of a pair. The third is process window. Resins formulated for very low loss are more tightly cross-linked, which raises drill wear, demands better oxide treatment at hybrid interfaces, narrows the lamination window and makes peel strength harder to hold.
On a 10-inch stripline at the 28 GHz Nyquist frequency of 112G PAM4:
| Stackup | Loss at 28 GHz (dB per inch) | 10-inch channel | Where it works |
|---|---|---|---|
| High-Tg FR-4 | 0.60 to 0.80 | 6 to 8 dB | Below 10 Gbps |
| Mid-loss FR-4 | 0.35 to 0.45 | 3.5 to 4.5 dB | 25 to 56 Gbps |
| Low-loss, Df under 0.005 | Below 0.30 | Under 3.0 dB | 112G with backdrill |
The board also has to fit more pairs per square centimetre each generation, which is where a dense stackup earns its place: HDI PCB​ builds with laser microvias let the escape routing leave a BGA without adding signal layers. Density and loss get reviewed together.
For a buyer, the ordering matters. Moving from high-Tg FR-4 to low-loss laminate is worth several decibels. Moving from low-loss to ultra-low loss is worth less than one in many channels, while backdrilling a connector via that resonates at 20 GHz is worth more than both. Spend on the stub first.
Heat changes the electrical answer
Temperature raises both Df and Dk, so the loss budget validated at room temperature is not the one the board runs at 90°C. Heat quietly rewrites the electrical answer.
The mechanism is molecular. As the resin warms, polar groups rotate more freely in the alternating field, relaxation polarization rises and the dielectric absorbs more energy per cycle. Absorbed moisture does the same more aggressively, since water has far higher loss than the polymer holding it. Published laminate data typically puts the Dk temperature coefficient between 200 and 400 ppm per degree Celsius for standard FR-4, around 100 to 200 for low-loss grades, and lower for PTFE and some ceramic-filled systems. Df moves the same way, commonly 20 to 40 percent higher between 25°C and 85°C on epoxy systems.
| Parameter | At 25°C | At 90°C | Effect on the channel |
|---|---|---|---|
| Dk | Datasheet value | Roughly 0.5 to 2 percent higher | Impedance drops about half that much |
| Df | Datasheet value | 20 to 40 percent higher | Dielectric loss rises at every frequency |
| Insertion loss | Validated value | Higher, mostly through Df | Eye height shrinks at the far end |
| Propagation delay | Nominal | Longer, since delay tracks the square root of Dk | Pair-to-pair timing needs rechecking |
The impedance relation is simple enough to use in review: a fractional change in Dk produces about half that change in impedance, in the opposite direction. Two percent more Dk is roughly one percent less impedance, a quarter of an eight percent band lost to temperature alone.
There is a feedback loop too. More loss means more heat along the trace, and more heat means more loss. That is small on one trace and much less small in a low-airflow corner beside a power stage, which is where accelerator boards put their densest routing.

The heat path a laminate cannot fix
The laminate is an insulator by design. Heat leaves the board through copper, in planes, via arrays, inlays and heavy copper, and only where copper geometry runs out does a different substrate make sense.
Glass-reinforced epoxy conducts 0.3 to 0.4 W/mK through the thickness. Copper conducts around 400. That gap is not a formulation problem the next grade will close; it is what the material is. Anisotropy matters as much as the number. Heat travels along glass fibres far better than across them, so a board spreads heat sideways more readily than it pushes heat from the top layer down to a cold plate. Spreading copper and via arrays under a die therefore do more than a slightly better resin.
What moves heat, in rough order of return: solid copper planes tied to the thermal path, via arrays under and around the hot package, copper inlays under the densest devices, and heavier copper on power layers. Where local heat flux still exceeds what those carry, the substrate has to change. A metal core PCB​ replaces the glass core with an aluminium or copper plate bonded through a thin thermally conductive dielectric, reaching 1 to 400 W/mK depending on the base, which suits a VRM cluster better than another two ounces of copper.
| Substrate | Through-thickness conductivity | Isolation | Cost position | Where it belongs |
|---|---|---|---|---|
| Standard FR-4 | 0.3 to 0.4 W/mK | Good | Baseline | Signal layers with moderate heat |
| High-Tg FR-4 | 0.4 to 0.5 W/mK | Good | Small premium | High-layer-count digital boards |
| Metal core | 1 to 400 W/mK | Set by the bond line | Moderate to high | Power stages, current-heavy modules |
| Ceramic, direct bonded copper | 20 to 230 W/mK | Above 3.5 kV | Highest | Power modules on high-voltage DC |
The last row matters more than it used to, because rack distribution is moving from 54 V to 800 V DC. That change puts isolation and thermal conduction in the same part, and a polymer dielectric has to trade one against the other. Ceramic does not.
Splitting the stackup instead of upgrading all of it
Put ultra-low-loss laminate only on the layers that carry the high-speed pairs, and keep high-Tg FR-4 on power, ground and structural layers. On a 20 to 30 layer accelerator board, only a handful of layers need the expensive dielectric.
This is how volume AI boards are actually built, and it is where pcb price gets decided. A typical split puts the low-loss material on four to eight inner signal layers, with high-Tg FR-4 everywhere else, including the thick copper planes and the outer layers that carry connectors.
| Layer group | Material | Why |
|---|---|---|
| SerDes pairs | Low-loss or ultra-low-loss | Carries the whole channel budget |
| Secondary signal layers | Mid-loss FR-4 | Short escapes where loss is not binding |
| Power and ground | High-Tg FR-4, heavy copper | Current capacity and heat spreading |
| Outer layers | High-Tg FR-4 | Mechanical strength, press-fit reliability |
Hybrid builds carry three risks. Tg and CTE mismatch can warp a large panel and load via barrels during reflow. The interface between two resin systems needs the right oxide or silane treatment, or peel strength drops and delamination shows up later. CAF has to be verified for the combination, not assumed from either datasheet. A symmetric build, matched prepreg and a lamination cycle written for the pair solve most of it, if the fabricator is asked before release.
What to lock before you release the stackup
Lock the test conditions, not just the material name. Two laminates with the same Df headline behave differently once frequency, method and copper finish are fixed.
| Item | Specify | Reason |
|---|---|---|
| Df and Dk | Frequency and test method | A 1 GHz value says little about 28 GHz |
| Dk tolerance | Per layer, not per panel | Impedance depends on the stack, not the average |
| Copper foil | Rz or profile grade | Conductor loss at 28 GHz is largely a foil decision |
| Via stub | Maximum residual length after backdrill | Stub resonance closes eyes faster than Df |
| Loss verification | S21 at operating temperature | The board runs hot, so check the budget hot |
| Thermal class | Tg, Td and T288 for the reflow profile | Heat resistance is separate from loss |

FAQ
Does a higher Tg laminate also have lower loss?​
No. Tg describes when the resin softens; Df describes how much energy it absorbs in an alternating field. They come from different parts of the formulation. A 180 °C FR-4 can sit near 0.016 Df while PTFE, with no meaningful transition in the operating range, sits under 0.002. Select for loss and thermal class separately.
Can you mix ultra-low-loss and standard FR-4 in one stackup?​
Yes, and most high-layer-count boards do. The work is in the interface: match CTE and Tg where the design allows, keep the build symmetric, specify prepreg for the pair, and verify CAF for the combination. Expect a tighter lamination window than either material needs alone.
Is a metal core board a drop-in replacement for a high-layer-count server board?​
No. Metal core boards typically run one to twelve layers with coarser routing, and the metal base is a heatsink rather than a signal reference. They solve local heat flux at a power stage. The high-speed pairs still belong on a low-loss laminate.